Effect of rotation speed and milling time to attain Nb10Hf1Ti .
WEBFeb 1, 2020 · The mechanical alloying process was performed in an argon atmosphere in the chamber and bullets of tungsten carbide with a balltopowder weight ratio (BPR) of 20:1 at rotation speed of 200, 300 and 400 rpm for 2, 5 and 8 h. At rotation speeds of 200 and 300 rpm particle size decreased and became more spherical during MA.